dc.contributor.author | Cetinkaya, Senol | |
dc.contributor.author | Eroglu, Serafettin | |
dc.date.accessioned | 2021-03-06T08:57:13Z | |
dc.date.available | 2021-03-06T08:57:13Z | |
dc.date.issued | 2012 | |
dc.identifier.citation | Cetinkaya S., Eroglu S., "Synthesis and reaction mechanism of Ti3SiC2 ternary compound by carbothermal reduction of TiO2 and SiO2 powder mixtures", CERAMICS INTERNATIONAL, cilt.38, ss.6445-6453, 2012 | |
dc.identifier.issn | 0272-8842 | |
dc.identifier.other | vv_1032021 | |
dc.identifier.other | av_e36a5a78-9942-4548-a2a0-cef5845100dd | |
dc.identifier.uri | http://hdl.handle.net/20.500.12627/149657 | |
dc.identifier.uri | https://doi.org/10.1016/j.ceramint.2012.05.020 | |
dc.description.abstract | The present study aims to investigate synthesis of Ti3SiC2 from TiO2 and SiO2 powder mixtures by carbothenrial reduction method. Equilibrium TiO2-SiO2-C ternary phase diagram was used to predict the conditions for the formation of Ti3SiC2 at 1800 K under Ar atmosphere. A reactant mixture with a TiO2:SiO2 molar ratio of 1.5 and a C content of 68.75 mol% (26.86 wt%) was initially selected among the thermodynamically favorable reactant compositions for the experimental studies. Two different C sources, graphite flakes and pyrolytic C coating, were used to synthesize Ti3SiC2 at 1800 K under Ar atmosphere. When graphite flakes were used, the products contained a trace amount of Ti3SiC2 phase along with major TiC and minor SiC phases. Whereas, pyrolytic C coating on the oxide particles resulted in the products with much higher Ti3SiC2 contents owing to the close contact between the reactants. Optimal C concentration for the C coated oxide mixtures with a TiO2:SiO2 molar ratio of 1.5 was determined to be 30.05 wt% under the experimental conditions studied. Ti3SiC2 content of the products obtained from this reactant was observed to increase with reaction time to 31 wt% at 75 min beyond which it gradually decreased. XRD studies indicated that the product with the highest ternary carbide content also contained TiC and a trace amount of SiC. SEM-EDS analyses showed that this sample essentially consisted of spherical fine TiC particles and Ti3SiC2 nanolaminates. Equilibrium thermodynamic analysis of the TiO2-SiO2-C system suggested that the reaction of solid Ti2O3 with SiO and CO gases may play a dominant role in the formation of Ti3SiC2. (c) 2012 Elsevier Ltd and Techna Group S.r.l. All rights reserved. | |
dc.language.iso | eng | |
dc.subject | MALZEME BİLİMİ, SERAMİK | |
dc.subject | Malzeme Bilimi | |
dc.subject | Mühendislik, Bilişim ve Teknoloji (ENG) | |
dc.subject | Mühendislik ve Teknoloji | |
dc.title | Synthesis and reaction mechanism of Ti3SiC2 ternary compound by carbothermal reduction of TiO2 and SiO2 powder mixtures | |
dc.type | Makale | |
dc.relation.journal | CERAMICS INTERNATIONAL | |
dc.contributor.department | İstanbul Üniversitesi , , | |
dc.identifier.volume | 38 | |
dc.identifier.issue | 8 | |
dc.identifier.startpage | 6445 | |
dc.identifier.endpage | 6453 | |
dc.contributor.firstauthorID | 29696 | |