dc.contributor.author | Oksuzomer, Mehmet Ali Faruk | |
dc.contributor.author | Sariboga, Vedat | |
dc.contributor.author | Ozdemir, Hasan | |
dc.date.accessioned | 2021-03-04T12:09:05Z | |
dc.date.available | 2021-03-04T12:09:05Z | |
dc.date.issued | 2013 | |
dc.identifier.citation | Sariboga V., Ozdemir H., Oksuzomer M. A. F. , "Cellulose templating method for the preparation of La0.8Sr0.2Ga0.83Mg0.17O2.815 (LSGM) Solid oxide electrolyte", JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, cilt.33, sa.8, ss.1435-1446, 2013 | |
dc.identifier.issn | 0955-2219 | |
dc.identifier.other | vv_1032021 | |
dc.identifier.other | av_75ead58c-6c8c-4b3d-93e4-7a9fb2ae17b4 | |
dc.identifier.uri | http://hdl.handle.net/20.500.12627/80983 | |
dc.identifier.uri | https://doi.org/10.1016/j.jeurceramsoc.2013.01.016 | |
dc.description.abstract | La0.8Sr0.2Ga0.83Mg0.17O2.815 (LSGM) materials are synthesized with a fast and facile cellulose templating method for the first time and characterized by XRD, EIS, Archimedes method and SEM-EDS. LSGM powders with a phase purity of 91.7 mol% are obtained after the calcination at 1300 degrees C for 12h. SEM-EDS results indicate possible decomposition and reconstruction of the LSGM phase due to the diffusion of Sr-rich species to the grain boundaries for the sample sintered at 1500 degrees C for 6 h. Maximum conductivity value is found to be 4.2 x 10(-2) S cm(-1) at 800 degrees C for the sample calcined at 1300 degrees C for 12 h and sintered at 1400 degrees C for 6 h. Phase purity, stability and relative density are the important factors for obtaining high performance LSGM electrolytes. Therefore, cellulose templating method is a promising candidate for the preparation of LSGM electrolytes. (C) 2013 Elsevier Ltd. All rights reserved. | |
dc.language.iso | eng | |
dc.subject | MALZEME BİLİMİ, SERAMİK | |
dc.subject | Mühendislik ve Teknoloji | |
dc.subject | Malzeme Bilimi | |
dc.subject | Mühendislik, Bilişim ve Teknoloji (ENG) | |
dc.title | Cellulose templating method for the preparation of La0.8Sr0.2Ga0.83Mg0.17O2.815 (LSGM) Solid oxide electrolyte | |
dc.type | Makale | |
dc.relation.journal | JOURNAL OF THE EUROPEAN CERAMIC SOCIETY | |
dc.contributor.department | İstanbul Üniversitesi , , | |
dc.identifier.volume | 33 | |
dc.identifier.issue | 8 | |
dc.identifier.startpage | 1435 | |
dc.identifier.endpage | 1446 | |
dc.contributor.firstauthorID | 70244 | |