dc.identifier.citationArabaci A., Sariboga V., Oksuzomer M. A. F. , "Er and Gd Co-Doped Ceria-Based Electrolyte Materials for IT-SOFCs Prepared by the Cellulose-Templating Method", METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, sa.11, ss.5259-5269, 2014
dc.identifier.issn1073-5623
dc.identifier.otherav_6237e45a-c3c6-4422-ad29-2c497126d6d6
dc.identifier.othervv_1032021
dc.identifier.urihttp://hdl.handle.net/20.500.12627/68411
dc.identifier.urihttps://doi.org/10.1007/s11661-014-2456-1
dc.description.abstractCe0.9-x Gd0.1Er (x) O1.9-x/2 (0 a parts per thousand currency sign x a parts per thousand currency sign 0.1) (EGDC) powders were successfully synthesized with a fast and facile cellulose-templating method for the first time and characterized by X-ray diffraction, scanning electron microscopy, and energy-dispersive X-ray spectroscopy. The samples were calcined at a relatively low calcination temperature of 773 K (500 A degrees C). The sintering behavior of the calcined EGDC powders was also investigated at 1673 K (1400 A degrees C) for 6 hours. Calcined Ce0.9-x Gd0.1Er (x) O1.9-x/2 (0 a parts per thousand currency sign x a parts per thousand currency sign 0.1) powders and sintered Ce0.9-x Gd0.1Er (x) O1.9-x/2 (0 a parts per thousand currency sign x a parts per thousand currency sign 0.1) pellets crystallized in the cubic fluorite structure. It was found that the relative densities of the sintered EGDC pellets were over 95 pct for all the Er contents studied. Moreover, the effect of Er content on the ionic conductivity of the gadolinium-doped ceria (GDC, Ce0.9Gd0.1O1.90) was investigated. The highest ionic conductivity value was found to be 3.57 x 10(-2) S cm(-1) at 1073 K (800 A degrees C) for the sintered Ce0.82Gd0.1Er0.08O1.91 at 1673 K (1400 A degrees C) for 6 hours.
dc.language.isoeng
dc.subjectMühendislik, Bilişim ve Teknoloji (ENG)
dc.subjectMALZEME BİLİMİ, MULTIDISCIPLINARY
dc.subjectMalzeme Bilimi
dc.subjectMETALURJİ VE METALURJİ MÜHENDİSLİĞİ
dc.subjectMetalurji ve Malzeme Mühendisliği
dc.subjectMühendislik ve Teknoloji
dc.titleEr and Gd Co-Doped Ceria-Based Electrolyte Materials for IT-SOFCs Prepared by the Cellulose-Templating Method
dc.typeMakale
dc.relation.journalMETALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE
dc.contributor.departmentİstanbul Üniversitesi , Mühendislik Fakültesi , Metelurji Ve Malzeme Mühendisliği
dc.identifier.issue11
dc.identifier.startpage5259
dc.identifier.endpage5269
dc.contributor.firstauthorID61926


Bu öğenin dosyaları:

DosyalarBoyutBiçimGöster

Bu öğe ile ilişkili dosya yok.

Bu öğe aşağıdaki koleksiyon(lar)da görünmektedir.

Basit öğe kaydını göster