dc.identifier.citationGumustas B., Dosdogru E. Y. , GÜNEYSU S., "EVALUATION OF MECHANICAL PROPERTIES OF FLUORIDE-RELEASING DENTAL MATERIALS AFTER MULTIPLE FLUORIDE RECHARGE/DISCHARGE APPLICATION", BIOSCIENCE JOURNAL, cilt.36, sa.4, ss.1461-1470, 2020
dc.identifier.issn1981-3163
dc.identifier.othervv_1032021
dc.identifier.otherav_5970259b-5444-4f3f-896b-4a91727521f6
dc.identifier.urihttp://hdl.handle.net/20.500.12627/62925
dc.identifier.urihttps://doi.org/10.14393/bj-v36n4a2020-47954
dc.description.abstractThis study aimed to determine the mechanical properties of fluoride-releasing dental materials after an accelerated fluoride recharge/discharge procedure. Two fluoride-releasing glass ionomer types of cement (Ketac Molar Easymix and IonoStar Molar), a resin-modified glass ionomer (Photac Fil Quick Aplicap), and two compomers (Compoglass F and Glasiosite) were used in this study. A total of 30 rectangular specimens and 30 disk specimens of each material were prepared and placed in distilled/deionized water (n = 5). The amount of fluoride released was analyzed from the materials for 7-day discharge, 1st recharge, 7-day discharge, 2nd recharge, and 7-day discharge, and 3rd recharge. The de/pre- and post-recharge fluoride release were measured using an ion chromatography for 24 days. The flexural strength and microhardness of each group were evaluated. The microhardness of all restorative materials showed no significant change (p > 0.05) over the experimental period. The flexural strength properties of the restorative materials did not change within the time of the study. The study showed that the fluoride release/uptake causes no effect on the mechanical and physical properties of dental materials.
dc.language.isoeng
dc.subjectFitopatoloji
dc.subjectBiyoteknoloji ve Genetik
dc.subjectToprak ve Bitki Besleme
dc.subjectToprak Verimliliği ve Gübreleme
dc.subjectTemel Bilimler
dc.subjectYaşam Bilimleri
dc.subjectTARIM, MULTİDİSİPLİNLER
dc.subjectTarım Bilimleri
dc.subjectTarım ve Çevre Bilimleri (AGE)
dc.subjectTARIM BİLİMİ
dc.subjectBİYOLOJİ
dc.subjectBiyoloji ve Biyokimya
dc.subjectYaşam Bilimleri (LIFE)
dc.subjectTıp
dc.subjectSağlık Bilimleri
dc.subjectTemel Tıp Bilimleri
dc.subjectBiyokimya
dc.subjectTıbbi Biyoloji
dc.subjectTarımsal Bilimler
dc.subjectZiraat
dc.subjectBitki Koruma
dc.titleEVALUATION OF MECHANICAL PROPERTIES OF FLUORIDE-RELEASING DENTAL MATERIALS AFTER MULTIPLE FLUORIDE RECHARGE/DISCHARGE APPLICATION
dc.typeMakale
dc.relation.journalBIOSCIENCE JOURNAL
dc.contributor.departmentİstanbul Medipol Üniversitesi , ,
dc.identifier.volume36
dc.identifier.issue4
dc.identifier.startpage1461
dc.identifier.endpage1470
dc.contributor.firstauthorID2284169


Bu öğenin dosyaları:

DosyalarBoyutBiçimGöster

Bu öğe ile ilişkili dosya yok.

Bu öğe aşağıdaki koleksiyon(lar)da görünmektedir.

Basit öğe kaydını göster