Basit öğe kaydını göster

dc.contributor.authorAl-mashhadani, Mukhallad M.
dc.contributor.authorUysal, Mucteba
dc.contributor.authorAYGÖRMEZ, Yurdakul
dc.contributor.authorCANPOLAT, Orhan
dc.date.accessioned2021-03-03T19:35:41Z
dc.date.available2021-03-03T19:35:41Z
dc.identifier.citationAYGÖRMEZ Y., CANPOLAT O., Al-mashhadani M. M. , Uysal M., "Elevated temperature, freezing-thawing and wetting-drying effects on polypropylene fiber reinforced metakaolin based geopolymer composites", CONSTRUCTION AND BUILDING MATERIALS, cilt.235, 2020
dc.identifier.issn0950-0618
dc.identifier.otherav_556e63f6-7059-4492-b2ee-a26644459f8b
dc.identifier.othervv_1032021
dc.identifier.urihttp://hdl.handle.net/20.500.12627/60390
dc.identifier.urihttps://doi.org/10.1016/j.conbuildmat.2019.117502
dc.description.abstractIn this study, metakaolin-based geopolymer samples produced by substitution of silica fume and cole-manite waste up to 20% were subjected to high-temperature effects at 300, 600, 900 degrees C, the wetting-drying effect of 5, 15 and 25 cycles and freezing-thawing effect of 56 and 300 cycles. At the end of the tests, compressive and flexural strengths, ultrasonic pulse velocity and weight changes' results were examined. In addition to these, micro-computed tomography (CT), XRD and SEM analyses were performed to examine the microstructure properties as well as visual inspection. 5 series produced for high temperature and wetting-drying effects were also produced with polypropylene fiber. It has been observed that samples exposed to 900 degrees C maintained their stability. Polypropylene fiber has been shown to increase the samples' flexural strength results compared to the non-fiber samples after exposing to high temperatures. For the freezing-thawing effect, air-entraining admixture was added to 5 series. An increase for compressive strength was seen after 56 cycles but a decrease was seen after 300 cycles. The geopolymer samples thus began to suffer the real distortion effect in subsequent cycles after the freezing-thawing effect, which contributed to geopolimerization in a sense occurring in the first 56 cycles. During the wetting-drying cycles, fluctuations were observed in the results and an increase in the compressive strength, UPV and weight changes' results after 5 cycles, a decrease in the results after 15 cycles and an increase again in the results after 25 cycles were seen. (C) 2019 Elsevier Ltd. All rights reserved.
dc.language.isoeng
dc.subjectMühendislik
dc.subjectMühendislik, Bilişim ve Teknoloji (ENG)
dc.subjectMÜHENDİSLİK, SİVİL
dc.subjectMALZEME BİLİMİ, MULTIDISCIPLINARY
dc.subjectMalzeme Bilimi
dc.subjectİnşaat Mühendisliği
dc.subjectYapı
dc.subjectMühendislik ve Teknoloji
dc.subjectİNŞAAT VE YAPI TEKNOLOJİSİ
dc.titleElevated temperature, freezing-thawing and wetting-drying effects on polypropylene fiber reinforced metakaolin based geopolymer composites
dc.typeMakale
dc.relation.journalCONSTRUCTION AND BUILDING MATERIALS
dc.contributor.departmentYıldız Teknik Üniversitesi , İnşaat Fakültesi , İnşaat Mühendisliği Bölümü
dc.identifier.volume235
dc.contributor.firstauthorID2277431


Bu öğenin dosyaları:

DosyalarBoyutBiçimGöster

Bu öğe ile ilişkili dosya yok.

Bu öğe aşağıdaki koleksiyon(lar)da görünmektedir.

Basit öğe kaydını göster