dc.identifier.citationKURUGÖL S., Gulec A., "PHYSICO-CHEMICAL, PETROGRAPHIC, AND MECHANICAL CHARACTERISTICS OF LIME MORTARS IN HISTORIC YOROS CASTLE (TURKEY)", INTERNATIONAL JOURNAL OF ARCHITECTURAL HERITAGE, cilt.6, sa.3, ss.322-341, 2012
dc.identifier.issn1558-3058
dc.identifier.otherav_2902a043-35f8-43e8-aa65-db16d4c65aa5
dc.identifier.othervv_1032021
dc.identifier.urihttp://hdl.handle.net/20.500.12627/32406
dc.identifier.urihttps://doi.org/10.1080/15583058.2010.540072
dc.description.abstractThis study examines the physicochemical, petrographic, and mechanical properties of lime mortars used in construction of Yoros Castle in the Byzantine period (13th-14th centuries AD). The study of mortar samples has been performed through polarizing and stereomicro-scope observations, x-ray diffraction (XRD) analyses, chemical (inductively coupled plasma emission spectroscopy [ICP-ES] and (high performance liquid chromatography [HPLC]), physical, and mechanical analyses. The hydraulic character of the mortars was mostly provided by pozzolanic brick dust and tuff additives. The results of spot tests indicate that the mortars contain protein and organic additives, which were used in their production. Albumin was detected during HPLC analysis, which was performed in order to determine the nature of the ingredients. The presence of albumin and vaterite, of which the latter was determined by XRD analysis, was considered to be the result of egg white content. The ignition loss and acid treatment analyses show that the binder/aggregate ratio varies between 1:2 and 1:3. The porosity ratio of mortars is approximately 30% on the average. According to the results of mechanical tests, average compressive strength of mortars is approximately 9.4 N/mm(2), flexural strength is approximately 2.4 N/mm(2). Despite their age of approximately 800 years, absence of extensive disintegration in the mortars may well indicate proper techniques of production.
dc.language.isoeng
dc.subjectSanat
dc.subjectİç Mimarlık
dc.subjectİnşaat Mühendisliği
dc.subjectYapı
dc.subjectMühendislik ve Teknoloji
dc.subjectMÜHENDİSLİK, SİVİL
dc.subjectSosyal ve Beşeri Bilimler
dc.subjectMühendislik, Bilişim ve Teknoloji (ENG)
dc.subjectMühendislik
dc.subjectİNŞAAT VE YAPI TEKNOLOJİSİ
dc.subjectSanat ve Beşeri Bilimler (AHCI)
dc.subjectSanat ve Beşeri Bilimler
dc.subjectMİMARİ
dc.titlePHYSICO-CHEMICAL, PETROGRAPHIC, AND MECHANICAL CHARACTERISTICS OF LIME MORTARS IN HISTORIC YOROS CASTLE (TURKEY)
dc.typeMakale
dc.relation.journalINTERNATIONAL JOURNAL OF ARCHITECTURAL HERITAGE
dc.contributor.departmentMimar Sinan Güzel Sanatlar Üniversitesi , ,
dc.identifier.volume6
dc.identifier.issue3
dc.identifier.startpage322
dc.identifier.endpage341
dc.contributor.firstauthorID202970


Files in this item

FilesSizeFormatView

There are no files associated with this item.

This item appears in the following Collection(s)

Show simple item record