dc.contributor.authorBeyaz, Rumeysa
dc.contributor.authorAYDIN, İSMAİL
dc.contributor.authorAtes, Murat
dc.contributor.authorÖKSÜZ, MUSTAFA
dc.contributor.authorYurtbasi, Zuhal
dc.contributor.authorEkinci, Aysun
dc.date.accessioned2023-02-21T09:17:59Z
dc.date.available2023-02-21T09:17:59Z
dc.identifier.citationBeyaz R., Ekinci A., Yurtbasi Z., ÖKSÜZ M., Ates M., AYDIN İ., "Thermal, electrical and mechanical properties of carbon fiber/copper powder/carbon black reinforced hybrid Polyamide 6,6 composites", HIGH PERFORMANCE POLYMERS, 2022
dc.identifier.issn0954-0083
dc.identifier.otherav_2bb477fd-dc32-4697-8574-5a74abbf327d
dc.identifier.othervv_1032021
dc.identifier.urihttp://hdl.handle.net/20.500.12627/187357
dc.identifier.urihttps://doi.org/10.1177/09540083221114752
dc.description.abstractThe development of low electrical and thermal properties of Polyamide (PA), which is used in place of metals in engineering applications, draws attention to the developments in various industrial disciplines. In this study, the effects of metal and carbon based fillers on the properties of Polyamide 6,6 (PA 6,6) were investigated. Especially, copper powder (Cu), carbon black (CB), carbon fiber (CF) and hybrid fillers (Cu/CB/CF) reinforced composites based on PA 6,6 were prepared by twin-screw extruder followed by injection molding. In the microstructure investigation, it was observed that the dispersion properties of used fillers were different in the PA 6,6 matrix. Both electrical and thermal conductivity of the PA 6,6 composites prepared were higher than pure PA 6,6. The highest electrical and thermal conductivity values were obtained as 7.97x 10(-2) S/cm and 0.73 W/mK for PA 6,6/CB30 and PA 6,6/CF/CB/Cu 10, respectively. The effects of the fillers on melting and crystallization behaviors and mechanical properties that affect the performance of PA 6,6 composites are also discussed. In general, the results showed that the mechanical properties of PA 6,6 composites were improved with the increase in the amount of hybrid filler. The highest tensile and notched Charpy impact strength were obtained as 252 MPa and 8.84 kJ/m(2) in PA 6,6 composite with 30% carbon fiber reinforcement by volume. As a result, the tensile properties of PA 6,6 hybrid composite were found to be superior to PA 6,6/CF composite with the same amount of carbon fiber content.
dc.language.isoeng
dc.subjectKimya (çeşitli)
dc.subjectPolimer Karakterizasyonu
dc.subjectTemel Bilimler
dc.subjectPolimerler ve Plastikler
dc.subjectFizik Bilimleri
dc.subjectGenel Kimya
dc.subjectPOLİMER BİLİMİ
dc.subjectKimya
dc.subjectTemel Bilimler (SCI)
dc.subjectFizikokimya
dc.titleThermal, electrical and mechanical properties of carbon fiber/copper powder/carbon black reinforced hybrid Polyamide 6,6 composites
dc.typeMakale
dc.relation.journalHIGH PERFORMANCE POLYMERS
dc.contributor.departmentYalova Üniversitesi , ,
dc.contributor.firstauthorID3439839


Files in this item

FilesSizeFormatView

There are no files associated with this item.

This item appears in the following Collection(s)

Show simple item record