dc.contributor.author | ARHUN, NESLİHAN | |
dc.contributor.author | Firatli, Erhan | |
dc.contributor.author | Ozel, Emre | |
dc.contributor.author | ATTAR, NURAY | |
dc.contributor.author | Firatli, Sonmez | |
dc.contributor.author | Gokcelik, Aylin | |
dc.contributor.author | ÖZEL, YONCA | |
dc.date.accessioned | 2021-03-06T20:29:57Z | |
dc.date.available | 2021-03-06T20:29:57Z | |
dc.date.issued | 2007 | |
dc.identifier.citation | Gokcelik A., ÖZEL Y., Ozel E., ARHUN N., ATTAR N., Firatli S., Firatli E., "The influence of Er : YAG laser conditioning versus self-etching adhesives with acid etching on the shear bond strength of orthodontic brackets", PHOTOMEDICINE AND LASER SURGERY, cilt.25, ss.508-512, 2007 | |
dc.identifier.issn | 1549-5418 | |
dc.identifier.other | av_fa72519c-8eae-416b-a202-3f52d156e58c | |
dc.identifier.other | vv_1032021 | |
dc.identifier.uri | http://hdl.handle.net/20.500.12627/163986 | |
dc.identifier.uri | https://doi.org/10.1089/pho.2007.2096 | |
dc.description.abstract | Objective: The aim of this study was to compare the shear bond strength (SBS) of orthodontic brackets after acid etching, laser ablation, self-etching primer application, and combined treatments. Methods: One hundred defect-free premolars were randomly assigned to five groups. The teeth received the following treatments: group 1: phosphoric acid + Transbond XT primer; group 2: Transbond Plus Self-Etching Primer (TPSEP); group 3: Er:YAG laser ablation + Transbond XT primer; group 4: Er:YAG laser ablation + phosphoric acid + Transbond XT primer; and group 5: Er:YAG laser ablation + TPSEP. Transbond XT Adhesive Paste was used in all groups for bracket bonding. Samples were stored in deionized water at 37 degrees C for 24 h. The shear debonding test was performed at a crosshead speed of 5 mm/min. Failed brackets were examined by a stereomicroscope at 16 X magnification to determine the bond failure interface using a modified adhesive remnant index (ARI). SBS values were compared using one-way analysis of variance (ANOVA). The Kruskal-Wallis test was used for ARI scores and pairwise comparisons were done using the Mann-Whitney U test with Bonferroni correction. Results: Mean SBS values (MPa) and standard deviations for the groups were: group 1, 13.18 +/- 3.45; group 2, 13.52 +/- 4.38; group 3, 10.33 +/- 4.74; group 41, 13.00 +/- 3.47; and group 5, 12.46 +/- 6.31. No significant differences were observed in the SBS of all the groups evaluated, but there was a significant difference in ARI scores, with group 3 showing higher ARI scores than groups 1 and 4. Conclusions: Er:YAG laser ablation and self-etching primer application showed similar SBS values as conventional acid-etching for bonding brackets. | |
dc.language.iso | eng | |
dc.subject | Klinik Tıp | |
dc.subject | Cerrahi Tıp Bilimleri | |
dc.subject | CERRAHİ | |
dc.subject | Sağlık Bilimleri | |
dc.subject | Tıp | |
dc.subject | Klinik Tıp (MED) | |
dc.title | The influence of Er : YAG laser conditioning versus self-etching adhesives with acid etching on the shear bond strength of orthodontic brackets | |
dc.type | Makale | |
dc.relation.journal | PHOTOMEDICINE AND LASER SURGERY | |
dc.contributor.department | Başkent Üniversitesi , , | |
dc.identifier.volume | 25 | |
dc.identifier.issue | 6 | |
dc.identifier.startpage | 508 | |
dc.identifier.endpage | 512 | |
dc.contributor.firstauthorID | 185493 | |