Basit öğe kaydını göster

dc.contributor.authorUlutas, Kemal
dc.contributor.authorBozoglu, Deniz
dc.contributor.authorArsu, Nergis
dc.contributor.authorDeger, Deniz
dc.contributor.authorYakut, Sahin
dc.contributor.authorAdibelli, Melisa
dc.contributor.authorCeper, Tolga
dc.date.accessioned2021-03-06T19:53:52Z
dc.date.available2021-03-06T19:53:52Z
dc.identifier.citationYakut S., Ulutas K., Bozoglu D., Adibelli M., Ceper T., Arsu N., Deger D., "Dielectric properties of AuNPs/PEGMEA/PEGDA nanocomposite film prepared with an alpha-amino ketone by in-situ photochemical method", PHYSICA B-CONDENSED MATTER, cilt.542, ss.6-11, 2018
dc.identifier.issn0921-4526
dc.identifier.othervv_1032021
dc.identifier.otherav_f863a791-b499-4c87-a9ce-6a31994f0dff
dc.identifier.urihttp://hdl.handle.net/20.500.12627/162713
dc.identifier.urihttps://doi.org/10.1016/j.physb.2018.04.037
dc.description.abstractDielectric properties and AC conductivity of in-situ formed AuNPs/PEGMEA/PEGDA nanocomposite film was investigated at room temperature. Frequency dependent dielectric constant shows that there are two main relaxation mechanisms for both samples. First of these mechanisms which correspond to dipolar polarization of long polymer chain was observed at frequencies between 0.1-10(3) Hz, 0.1-10(4) Hz for PEGMEA/PEGDA film and AuNPs/PEGMEA/PEGDA nanocomposite film, respectively. This mechanism has dielectric constant of 10.8, 14.1 for PEGMEA/PEGDA film and AuNPs/PEGMEA/PEGDA nanocomposite film, respectively. The second mechanism which was attributed to dipolar polarization of chain branches was observed at frequencies between 10(2)-10(6) Hz, 10(5)-10(7) Hz for PEGMEA/PEGDA film and AuNPs/PEGMEA/PEGDA nanocomposite film, respectively. This mechanism has dielectric constant of 9.6 for PEGMEA/PEGDA film and 10.3 for AuNps/PEGMEA/PEGDA nanocomposite film which cured in the presence of Irg-907 as Type I initiator by using medium pressure mercury light. These relaxation mechanisms can also be detected at frequency dependence of dielectric dissipation (tan delta) as Cole-Cole fitted relaxation peaks and of AC conductivity graphs as frequency independent (DC-like), and frequency dependent regions. DC-like region, it was thought that the main effect of AuNPs was observed, has values for AuNPs/PEGMEA/PEGDA nanocomposite film and PEGMEA/PEGDA film as 6x10(-7) and 2x10(-8) S/cm, respectively. In addition to these two polarization mechanisms, electrode polarization was observed at frequencies lower than 1 Hz for AuNps/PEGMEA/PEGDA nanocomposite film due to accumulation of AuNPs.
dc.language.isoeng
dc.subjectFizik
dc.subjectTemel Bilimler
dc.subjectFİZİK, YOĞUN MADDE
dc.subjectYoğun Madde 1:Yapısal, Mekanik ve Termal Özellikler
dc.subjectTemel Bilimler (SCI)
dc.titleDielectric properties of AuNPs/PEGMEA/PEGDA nanocomposite film prepared with an alpha-amino ketone by in-situ photochemical method
dc.typeMakale
dc.relation.journalPHYSICA B-CONDENSED MATTER
dc.contributor.departmentYıldız Teknik Üniversitesi , ,
dc.identifier.volume542
dc.identifier.startpage6
dc.identifier.endpage11
dc.contributor.firstauthorID2175548


Bu öğenin dosyaları:

DosyalarBoyutBiçimGöster

Bu öğe ile ilişkili dosya yok.

Bu öğe aşağıdaki koleksiyon(lar)da görünmektedir.

Basit öğe kaydını göster