dc.identifier.citationIyim T., Ozgumus S., Orbay M., "Blends and reaction products prepared from phenolic resin and waste PET. II. Thermal oxidative degradation", POLYMER-PLASTICS TECHNOLOGY AND ENGINEERING, cilt.42, ss.17-32, 2003
dc.identifier.issn0360-2559
dc.identifier.otherav_cade6162-e207-479f-b055-8a63c21c51dd
dc.identifier.othervv_1032021
dc.identifier.urihttp://hdl.handle.net/20.500.12627/134402
dc.identifier.urihttps://doi.org/10.1081/ppt-120016333
dc.description.abstractHigh ortho novolactype phenolic resin and waste poly(ethylene terephthalate) (PET) were used to prepare blends and reaction products. The effect of PET on the thermal oxidative stability of these products was investigated with thermogravimetric analysis (TGA), differential scanning calorimetry (DSC), and fourier transform infrared spectroscopy (FTIR). It was determined that presence of PET in blends improved the stability and in case of reaction products, degradation was prevented up to 370degreesC.
dc.language.isoeng
dc.subjectTemel Bilimler (SCI)
dc.subjectPolimer Karakterizasyonu
dc.subjectPOLİMER BİLİMİ
dc.subjectKimya
dc.subjectFizikokimya
dc.subjectTemel Bilimler
dc.titleBlends and reaction products prepared from phenolic resin and waste PET. II. Thermal oxidative degradation
dc.typeMakale
dc.relation.journalPOLYMER-PLASTICS TECHNOLOGY AND ENGINEERING
dc.contributor.department, ,
dc.identifier.volume42
dc.identifier.issue1
dc.identifier.startpage17
dc.identifier.endpage32
dc.contributor.firstauthorID166828