dc.identifier.citationGunay V., Gelecek-Sulan O., Ozkan O., "Grain growth kinetic in xCoO-6 wt.% Bi2O3-(94-x) ZnO (x = 0, 2, 4) ceramic system", CERAMICS INTERNATIONAL, cilt.30, ss.105-110, 2004
dc.identifier.issn0272-8842
dc.identifier.otherav_97031f95-66a1-4b98-ab17-84c74f44d6c7
dc.identifier.othervv_1032021
dc.identifier.urihttp://hdl.handle.net/20.500.12627/101654
dc.identifier.urihttps://doi.org/10.1016/s0272-8842(03)00071-3
dc.description.abstractThe grain growth kinetics in the 0, 2, 4 wt.% CoO added ZnO-6 wt.% Bi2O3 system was studied using the simplified phenomenological grain growth kinetics equation G(n) = K.t.exp(-Q/RT) together with the physical properties of the sintered samples. The grain growth exponent value (n) and the apparent activation energy for the ZnO-6 wt.% Bi2O3 system was found to be 5.2 and similar to200 kJ/mol respectively. The addition of the CoO to the ZnO-6 wt.% Bi2O3 system had no effect in the grain growth. At 0% CoO addition the apparent activation energy was calculated as 204 kJ/mol and with 4 wt.% CoO addition it was calculated as 203 kJ/mol. (C) 2003 Elsevier Ltd and Techna S.r.l. All rights reserved.
dc.language.isoeng
dc.subjectMALZEME BİLİMİ, SERAMİK
dc.subjectMühendislik ve Teknoloji
dc.subjectMühendislik, Bilişim ve Teknoloji (ENG)
dc.subjectMalzeme Bilimi
dc.titleGrain growth kinetic in xCoO-6 wt.% Bi2O3-(94-x) ZnO (x = 0, 2, 4) ceramic system
dc.typeMakale
dc.relation.journalCERAMICS INTERNATIONAL
dc.contributor.department, ,
dc.identifier.volume30
dc.identifier.issue1
dc.identifier.startpage105
dc.identifier.endpage110